Results 61 to 70 of about 49,671 (256)

Unified fracture criterion for brittle 2D materials

open access: yesnpj Computational Materials
Two-dimensional materials (2DMs), possessing atomic-scale thickness, are prone to brittle fracture under loading conditions, which can lead to catastrophic failure.
Shenda Jiang   +5 more
doaj   +1 more source

Design and manufacturing of abrasive jet machine for drilling operation

open access: yesMATEC Web of Conferences, 2016
Wide application of Abrasive Jet Machine (AJM) is found in machining hard and brittle materials. Machining of brittle materials by AJM is due to brittle fracture and removal of micro chips from the work piece.
Mittal Divyansh   +2 more
doaj   +1 more source

Creep Properties and Deformation Mechanism of Additively Manufactured NiAl‐CrMo Composites

open access: yesAdvanced Engineering Materials, EarlyView.
Additively manufactured NiAl‐CrMo composites contain numerous interfaces and cell boundaries that control their creep response. At 700°C under high applied stress, creep is dominated by dislocation‐controlled power‐law mechanisms. At 800°C–900°C and lower stresses, creep is primarily diffusion‐controlled along cell boundaries.
Jan Vollhüter   +9 more
wiley   +1 more source

Comparison of Triply Periodic Minimal Surface Energy Absorbers Under Uniaxial Compressive Loading

open access: yesAdvanced Engineering Materials, EarlyView.
This study investigates LCD 3D printed Triply Periodic Minimal Surface (TPMS) structures as mechanical energy absorbers. By comparing various base designs and layered combinations under uniaxial compression, it identifies that a Diamond‐Gyroid sandwich structure offers superior performance.
Sergej Grednev   +2 more
wiley   +1 more source

“7M”Advantage of Abrasive Waterjet for Machining Advanced Materials

open access: yesJournal of Manufacturing and Materials Processing, 2017
Under the support of an SBIR Phase II/IIB grant from the National Science Foundation, OMAX has developed and commercialized micro abrasive (µAWJ), culminating A MicroMAX® JetMachining® Center technology for meso-micro machining.
(Peter) H.-T. Liu
doaj   +1 more source

Additive Manufacturing of Alumina‐Reinforced Elastomers

open access: yesAdvanced Engineering Materials, EarlyView.
Vat‐photopolymerized elastomers reinforced with platelet‐shaped alumina exhibited preferential orientation, reduced porosity, and significantly enhanced mechanical performance. A 3 wt% platelet loading increased tensile strength from 12.4 to 45.7 MPa, highlighting the critical role of filler morphology in elastomeric VPP composites.
Majid Barzegar Keyvani   +6 more
wiley   +1 more source

Research progress on laser joining of brittle and transparent materials

open access: yesHanjie xuebao
The joining technology of brittle and transparent materials has been widely applied in aerospace, electronic packaging, and sensor industries. Research on the joining technology of transparent materials holds significant academic and engineering ...
Rui PAN   +6 more
doaj   +1 more source

A Review on Brittle Fracture Nanomechanics by All-Atom Simulations

open access: yesNanomaterials, 2019
Despite a wide range of current and potential applications, one primary concern of brittle materials is their sudden and swift collapse. This failure phenomenon exhibits an inability of the materials to sustain tension stresses in a predictable and ...
Sandeep P. Patil, Yousef Heider
doaj   +1 more source

High‐Temperature Phase Transformation in a V‐9Si‐6.5B Alloy: The Kinetic and Crystallographic Pathway From V5SiB2 to V8SiB4

open access: yesAdvanced Engineering Materials, EarlyView.
In situ synchrotron high‐energy X‐ray diffraction reveals the real‐time high‐temperature phase evolution of a ternary V‐9Si‐6.5B alloy. The study uncovers a kinetically delayed V5SiB2 → V8SiB4 transformation governed by massive structural and chemical barriers.
Zahra Sabeti   +4 more
wiley   +1 more source

Impact of MgO Additions on the Oxidation Resistance and Compression Behavior of Vanadium Alloys

open access: yesAdvanced Engineering Materials, EarlyView.
An increase in oxidation resistance at 600 °C is achieved for alloys containing more than 2.5 wt.% MgO. It has been established that, along with V2O5, MgO6V2, and Mg2O7V2 are formed, which are presumed to enhance oxidative stability. Furthermore, the possible transformation of Mg‐vanadates through reaction with CO2, which presumably occurs in this ...
Ievgen Solodkyi   +5 more
wiley   +1 more source

Home - About - Disclaimer - Privacy