Results 51 to 60 of about 1,086,234 (300)

Major spinal surgery procedure on a high cardiovascular risk patient with symptomatic neural compression due to 1: Osteoporotic T12 compression fracture along with 2—L5/S1 spondylolisthesis

open access: yesJournal of Spinal Surgery, 2014
Introduction: Osteoporotic vertebral fracture most common located at thoracolumbar junction, whereas most spondylolisthesis at L4-5 is six to 10 times more frequent involved than adjacent level.
Sumeet G Pawar   +2 more
doaj   +1 more source

Prognostic Factors of Percutaneous Vertebroplasty for Vertebral Compression Fracture and Risk Factors of New Symptomatic Compression Fracture

open access: yesFormosan Journal of Musculoskeletal Disorders, 2023
Background: Vertebral compression fractures (VCFs) are a common complication of osteoporosis and can lead to severe pain, decreased mobility, and reduced quality of life. Percutaneous vertebroplasty (PVP) is an effective minimally invasive procedure used
Wen-Chien Wang   +6 more
doaj   +1 more source

Causes of scatter in high rate fracture testing of polymers [PDF]

open access: yes, 2013
A method based on the measurement of failure time is being developed by the European Structural Integrity Society to determine high rate fracture toughness of polymers.
Horsfall I.   +3 more
core   +1 more source

Buckling And Fracture Analysis Of Thick And Long Composite Cylinders With Cutouts Under Axial Compression: An Experimental And Numerical Campaign

open access: yes, 2023
This article reports on the manufacturing, experimental testing, and finite element analysis of very thick and long carbon-fiber-reinforced polymers (CFRP) tubes under uniaxial compression (radius-to-thickness ratio ∼ 10 and length-to-radius ratio ∼ 21).
I.E. Tabrizi   +20 more
core   +1 more source

A Numerical–Experimental Approach for Multi‐Matrix Fiber‐Reinforced Plastics Characterization Using Finite Element Model Updating

open access: yesAdvanced Engineering Materials, EarlyView.
A numerical–experimental framework is developed for characterizing multi‐matrix fiber‐reinforced polymers (MM‐FRPs) combining epoxy and polyurethane matrices. Harmonic bending tests are integrated with finite element model updating (FEMU) to simultaneously identify elastic and viscoelastic material parameters.
Rodrigo M. Dartora   +4 more
wiley   +1 more source

Flexural Behavior of 3D‐Printed Porous Bouligand‐Structured Polymers: Influence of Pitch Angle and Porosity

open access: yesAdvanced Engineering Materials, EarlyView.
This study examines how helicoidal architectures with different porosities respond to bending. Adjusting layer angle and spacing in 3D‐printed polymers reveals clear tradeoffs between stiffness, strength, and energy absorption. Experiments and simulations highlight designs that distribute stress effectively, offering pathways for optimizing lightweight
Praveenkumar Subhash Patil   +2 more
wiley   +1 more source

Compression-shear fracture and energy evolution in rock-like materials under hydraulic-mechanical coupling effect

open access: yesGeomechanics and Geophysics for Geo-Energy and Geo-Resources
The mechanical behavior of fractured rock masses under the operation of hydraulic-mechanical coupling is of enormous practical relevance, and the failure process gives theoretical support for disaster avoidance and mitigation of high hydraulic pressure ...
Taoying Liu   +5 more
doaj   +1 more source

Chest X-Ray Assessment is Incomplete without the Lateral View [Letter]

open access: yesAdvances in Medical Education and Practice, 2021
Bruce Rothschild IU Health, Muncie, IN 47303, USACorrespondence: Bruce RothschildIU Health, Muncie, IN 47303, USATel +1-7856151523Email Spondylair@gmail.comThe article by Sait and Tombs1 represents an important contribution to the preparation of ...
Rothschild B
doaj  

Electrochemical Behavior of Flame‐Sprayed Sc‐Doped AlCoCrFeMo High‐Entropy Alloy Coatings in 3.5% Sodium Chloride Solution

open access: yesAdvanced Engineering Materials, EarlyView.
Scandium (Sc)‐doped AlCoCrFeMo HEA coatings are fabricated via flame spraying with 0.1, 0.3, and 0.5 wt% Sc additions. Among these, the HEA‐Sc0.3 coating exhibits the highest corrosion resistance, indicated by a more positive corrosion potential and lower current density.
Pankaj Kumar   +7 more
wiley   +1 more source

Crack initiation and fracture features of Fe–Co–B–Si–Nb bulk metallic glass during compression [PDF]

open access: yesFracture and Structural Integrity, 2016
The aim of the paper was investigation crack initiation and fracture features developed during compression of Fe-based bulk metallic glass (BMG). These Fe-based BMG has received great attention as a new class of structural material due to an excellent ...
S. Lesz   +3 more
doaj  

Home - About - Disclaimer - Privacy