Results 131 to 140 of about 514,656 (304)

Synthesis of a Novel Thermoresponsive S53P4 Bioactive Glass Extract–Poloxamer 407 Injectable Hydrogels: Assessment of Biocompatibility and Antimicrobial Properties

open access: yesAdvanced Engineering Materials, EarlyView.
This study investigates innovative thermoreversible hydrogels derived from S53P4 bioactive glass extracts to aid in the healing of infected diabetic foot wounds. These injectable gels, which gel at body temperature, release beneficial ions and remain stable over time.
Marian G. Vargas Guerrero   +9 more
wiley   +1 more source

The use of enteral access for continuous delivery of levodopa-carbidopa in patients with advanced Parkinson's disease. [PDF]

open access: yesUnited European Gastroenterol J, 2017
Cheron J   +11 more
europepmc   +1 more source

Prediction of Surface Topography Parameters in Direct Laser Interference Patterning of Stainless Steel Using Infrared Monitoring and Convolutional Neural Networks

open access: yesAdvanced Engineering Materials, EarlyView.
This study presents an infrared monitoring approach for direct laser interference patterning (DLIP) combined with a convolutional neural network (CNN). Thermal emission data captured during structuring are used to predict surface topography parameters.
Lukas Olawsky   +5 more
wiley   +1 more source

Interaction between Molten Al‐Killed Mn–B Steel and Carbon‐Bonded MgO Refractories Based on Recyclates

open access: yesAdvanced Engineering Materials, EarlyView.
High‐temperature interactions between low‐sulfur Al‐killed Mn–B steel and MgO–C refractories (0 and 50 wt% recyclates) are studied via finger immersion tests (1600 °C). Surface‐active elements influence infiltration. MgO/CaS layer forms, along with spinel and calcium silicate.
Matheus Roberto Bellé   +5 more
wiley   +1 more source

Characterization of Nitinol Produced by Laser Powder Bed Fusion for Mechanical Metamaterial Applications

open access: yesAdvanced Engineering Materials, EarlyView.
Stabilization of L‐PBF Ni50.7Ti49.3 under low‐cycle loading was investigated. Recoverable strain after cycling was dependent on the amount of applied load. Recovery ratio was 53.4% and 35.1% at intermediate and high load, respectively. The maximum total strain reached 10.3% at a high load of 1200 MPa.