Vat photopolymerization debinding exhibits complex behavior depending on layer-by-layer deposition, scraping, lasing conditions, anisotropy of shrinkage, polymer decomposition, and shape thickness environments, making debinding cracks difficult to ...
Charles Manière +2 more
doaj +1 more source
Digital light processing of yttria-stabilized zirconia: Modeling photoinitiator decay
A digital process was developed to facilitate additive manufacturing for ceramic materials using digital light processing (DLP). A numerical model that predicts DLP sample properties can be generated from manufacturing inputs to forecast the effect of ...
Brennan Harris +3 more
doaj +1 more source
Fused Deposition Modeling and Mechanical Properties of Porous Titanium Scaffolds
To address issues such as thermal stress concentration in metal bone implants produced via high-energy beam direct additive manufacturing, a method was proposed to fabricate porous titanium scaffolds. This approach combined Fused Deposition Modeling (FDM)
Suli Li, Zhijie Guo, Yang Gao, Jing Guo
doaj +1 more source
Impact of oxygen content on debinding of binder jetted 17-4 PH stainless steel: Part I – Debinding
Binder jetting (BJT) utilises a sacrificial binder to shape green parts in a metal powder bed. The binder must be removed during debinding at elevated temperatures without contaminating the powder material. Efficient binder removal often requires oxygen in the atmosphere to aid the decomposition of the binder, but oxygen causes ...
Kai Zissel +3 more
openaire +1 more source
As additive manufacturing gains widespread adoption across various industries, its application to traditional materials such as bronze remains relatively underexplored.
Xueying Wei +3 more
doaj +1 more source
In advanced powder metallurgy technologies such as metal injection molding (MIM) and material extrusion technology (MEX), the intricate synergy between binder components and metallic powders within feedstocks is predominant, dictating the technological ...
Cristina Berges +2 more
doaj +1 more source
Toshiki Nakamura +2 more
openaire +2 more sources
Progress in Characterizing Curing and Debinding of Ceramic Inks for Stereolithography
ABSTRACT During ceramic stereolithography, laser photopolymerization must achieve high and uniform curing of monomers to ensure a crack‐free debinding step. In this study, we present a spatially resolved quantification of curing rate using Fourier transform infrared (FTIR) spectroscopy, relying on advanced deconvolution methods ...
Sylvain Fournier +3 more
openaire +1 more source
Debinding Behavior for Injection Molded Alumina Compacts.
A thermal treatment causes occasionally some defects for green body like cracks or blisters in a binder removal stage of the ceramic injection molding process.A debinding mechanism by heating for the injection molded alumina contained the EVA and Wax is investigated in this study.
openaire +2 more sources
Post-Processing Optimization of MDLP-Fabricated 316L Stainless Steel: Microstructural Evolution and Mechanical Properties. [PDF]
Wu Z +8 more