Results 1 to 10 of about 645,605 (160)
Experimental and numerical analyses of magnesium alloy hot workability [PDF]
Due to their hexagonal crystal structure, magnesium alloys have relatively low workability at room temperature. In this study, the hot workability behavior of cast-extruded AZ31B magnesium alloy is studied through hot compression testing, numerical ...
Fethi Abbassi +2 more
exaly +4 more sources
Revealing the grain size dependent hot workability and deformation mechanisms in a Mg-Zn-Y alloy
Despite the industrial significance of grain size for enhancing mechanical properties and formability, the in-depth deformation mechanisms at elevated temperature are still unclear.
Fulin Jiang, Hui Zhang, Jie Teng
exaly +4 more sources
Hot workability of nanocrystalline AZ91 magnesium alloy [PDF]
This study examined the hot deformation behavior and workability characteristics of nanocrystalline AZ91 Mg alloy by performing hot compression tests with a Gleeble-3800 machine. To this end, a nanocrystalline alloy powder with a crystallite size of 25 nm was synthesized via mechanical milling of a pre-alloyed AZ91 Mg alloy powder for 14 h.
Jabbari Taleghani, Mohammad Ali +1 more
exaly +5 more sources
The effect of the initial powder particle size on the hot workability of Ni-based superalloys was investigated. Herein, four powders with different particle size ranges (106 μm) exhibited superior hot workability than that of the sample fabricated using ...
Masaya Higashi
exaly +3 more sources
The conditions for increasing the hot workability and extending the temperature range for the safe hot working of M2 high-speed steel (HSS) were studied and revealed. This was enabled by combination of two approaches, i.e. results obtained by an analysis
Iztok Peruš +3 more
doaj +2 more sources
This paper investigates the impact of pre-precipitated η phases and Al3(Er, Zr) particles on the hot workability and recrystallization behavior of an Al–Zn–Mg–Er–Zr alloy. The optimal pre-precipitation heat treatment prior to hot deformation was obtained
Wu Wei, Shengping Wen, Jiongshen Chen
exaly +3 more sources
Hot Workability of 5052 Aluminum Alloy
Gavgali, M., Totik, Y.
openaire +2 more sources
Hot deformation behavior of micro-alloyed steel using processing maps developed with different constitutive equations [PDF]
The hot workability of microalloyed steel was studied in the deformation temperature range of 850–1200ºC and strain rate of 0.001-100s-1. The constitutive relation of flow stress with temperature, strain rate and strain was established to construct ...
Thakur S.K., Das A.K., Jha B.K.
doaj +1 more source
Hot workability and microstructural evolution of Ti-5.5Al-5Mo-5V-2Nb-1Fe-1Zr titanium alloy, which is also called Ti555211 titanium alloy, are investigated during compressive deformation at different temperatures and strain rates.
Yushe Gao +8 more
doaj +1 more source
Hot Working of an Fe-25Al-1.5Ta Alloy Produced by Laser Powder Bed Fusion
In the present work, hot working was used as a post-processing method for Fe-25Al-1.5Ta (at.%) alloy built using laser powder bed fusion (LPBF) to refine the undesirable columnar microstructure with heterogeneous grain sizes and strong textures in the ...
Aliakbar Emdadi +2 more
doaj +1 more source

