Results 181 to 190 of about 530,601 (300)

Hydrogen‐Assisted Fracture of Iron‐Based Fe–Ni–Al Alloys

open access: yesAdvanced Engineering Materials, EarlyView.
Principal relations and fracture mechanisms of single‐phase and precipitate‐strengthened Fe–Ni–Al alloys subjected to prior electrochemical hydrogen charging are identified. The mechanisms of hydrogen effect on strength and microhardness are discussed, including hydrogen‐induced increase in microhardness and the role of hydrogen in fracture behavior ...
Nataliya Yadzhak   +3 more
wiley   +1 more source

Dual Pathways Coupled to Oxytocin Molecular Signals in Cultured Astrocytes. [PDF]

open access: yesCells
Farsetti E   +11 more
europepmc   +1 more source

Influence of Test Temperature and Test Frequency on Fatigue Life of Aluminum Alloy EN AW‐2618A

open access: yesAdvanced Engineering Materials, EarlyView.
The influence of test temperature and test frequency on the fatigue life of EN AW‐2618A is investigated. High‐cycle fatigue tests are performed at different test temperatures and frequencies on the 1000 h/230°C overaged state. Both test parameters reduce fatigue life due to time‐dependent damage mechanisms.
Ying Han   +5 more
wiley   +1 more source

Interaction of Human Lymphocyte Scavenger Receptors CD5 and CD6 with Toxins from <i>Naja haje</i>, <i>Androctonus australis</i> and <i>Apis mellifera</i> Venoms. [PDF]

open access: yesBiomolecules
Khemili D   +9 more
europepmc   +1 more source

Electrochemical Behavior of Flame‐Sprayed Sc‐Doped AlCoCrFeMo High‐Entropy Alloy Coatings in 3.5% Sodium Chloride Solution

open access: yesAdvanced Engineering Materials, EarlyView.
Scandium (Sc)‐doped AlCoCrFeMo HEA coatings are fabricated via flame spraying with 0.1, 0.3, and 0.5 wt% Sc additions. Among these, the HEA‐Sc0.3 coating exhibits the highest corrosion resistance, indicated by a more positive corrosion potential and lower current density.
Pankaj Kumar   +7 more
wiley   +1 more source

Experimental Characterization and Constitutive Modeling of the Effect of Prior Inelastic Strain on the Viscoplastic Behavior of AD730 at 700 °C

open access: yesAdvanced Engineering Materials, EarlyView.
This study shows that superalloys used in aircraft engine disks become much more prone to deformation at high temperatures if they have been strained during manufacturing. This effect increases with the level of prior strain but eventually reaches a limit.
Fabio Machado Alves da Fonseca   +9 more
wiley   +1 more source

Advanced Electron Microscopy and Microcomputed Tomography Analysis of Single‐Crystal Ni‐Base Superalloys After Short‐Term Multiaxial Creep

open access: yesAdvanced Engineering Materials, EarlyView.
This work studies the anisotropic behavior of circular notched tensile specimens of Ni‐base superalloy single crystals during high‐temperature tensile creep along [001], [110], and [111]. Correlative scale‐bridging imaging of specimens reveals early rupture along [110] because 1) plastic deformation proceeds faster at notch center; 2) more (brittle ...
Leonardo Agudo Jácome   +6 more
wiley   +1 more source