Effect of Solidification Direction on the Freckle Formation in Single-Crystal Superalloy Castings. [PDF]
Ma D +13 more
europepmc +1 more source
Single-Crystal Inspection Using an Adapted Total Focusing Method. [PDF]
Aizpurua-Maestre I +4 more
europepmc +1 more source
Spherical Indentation Behavior of DD6 Single-Crystal Nickel-Based Superalloy via Crystal Plasticity Finite Element Simulation. [PDF]
Hao X +7 more
europepmc +1 more source
Anisotropy in Creep Behavior of a Directionally Solidified Ni-Based Superalloy at 980 °C and 1070 °C. [PDF]
Long A +6 more
europepmc +1 more source
Surface Topography of Hardened Stainless Steel in Dry Finish Turning Using CBN and Cemented Carbide Inserts. [PDF]
Leksycki K, Feldshtein E, Pawłowski J.
europepmc +1 more source
Type-I hot corrosion behavior of Cr-modified slurry aluminide coating superalloy Rene 80. [PDF]
Shirvani K +3 more
europepmc +1 more source
Creep Mechanism and Microstructure Evolution of a Directionally Solidified Ni-Based Superalloy with Different Orientations at 850 °C. [PDF]
Long A +6 more
europepmc +1 more source
Multi-Phase Design Strategy for Synergistic Strength-Ductility Optimization in V-Ti-Cr-Nb-Mo Refractory High-Entropy Alloys. [PDF]
Liang X +5 more
europepmc +1 more source
Hot Deformation Behavior and Microstructure Evolution of a Fe-Ni-Cr Based Superalloy. [PDF]
Wang Y +8 more
europepmc +1 more source