Recrystallisation of single crystal superalloy CMSX–4

Materials Science and Technology, 2003
AbstractA series of experiments investigating the recrystallisation of single crystal superalloy CMSX-4 have been carried out. Indentation atroom temperature has been used to study the effects of annealing time and temperature, and it has been found that a very strong dependence upon temperature is evident.
D. C. Cox   +3 more
openaire   +1 more source

Directionally Solidified and Single-Crystal Superalloys

1990
Abstract Directionally solidified (DS) and single-crystal (SX) superalloys and process technology are contributing to significant advances in turbine engine efficiency and durability. These gains are expected to arise from the development of higher creep strength and improved oxidation-resistant SX alloy compositions as well as from the ...
K. Harris, G.L. Erickson, R.E. Schwer
openaire   +1 more source

Single Crystal Superalloys

Advanced materials such as single crystal superalloys (SCSs) are made especially for high temperature uses, including turbine engines in the aerospace and electricity generation companies. Their single crystalline shape, which distinguishes their microstructures, confers superior mechanical behaviours, including remarkable fatigue strength and creep ...
openaire   +2 more sources

Anisotropic Creep of Single Crystal Superalloys

2001
Single crystal Ni-base superalloys are an integral feature of modern gas turbine engines. Their excellent high temperature tensile properties are a result of a number of factors including an absence of grain boundaries and a matrix which comprises a high volume fraction of cuboidal γ’ in a solid solution strengthened γ matrix.
D. M. Knowles, D. W. MacLachlan
openaire   +1 more source

Segregation in Single-Crystal Nickel-Base Superalloys

Defect and Diffusion Forum, 2011
The effect and the ways of removal of the segregation of alloying elements within the dendrite cell in single-crystal nickel-base superalloys are discussed. The peculiar features of Re and Ru behavior are underlined.
A.I. Epishin   +4 more
openaire   +1 more source

HIGH TEMPERATURE FATIGUE IN SINGLE CRYSTAL SUPERALLOYS

Fatigue & Fracture of Engineering Materials & Structures, 1997
Abstract— The growth rate of fatigue cracks in two single crystal nickel base superalloys, CMSX‐6 and SRR99, along the <001> planes are presented and rationalised in terms of two interacting crack propagation mechanisms: one attributed to crack tip plastic blunting and the other attributed to the brittle failure of the oxide scales.
J. M. Martínez‐Esnaola   +4 more
openaire   +1 more source

Recycled Applications of a Single Crystal Superalloy

Advanced Materials Research, 2011
The effects of application of recycled scraps on the composition, microstructure and mechanical properties of SRR99 alloy were studied. The compositions of recycle master alloy are similar to that of the fresh alloy. However, nitrogen content, the size and amount of microporosity increase significantly with the recycle material proportion.
Jin Jiang Yu   +5 more
openaire   +1 more source

Strengthening Mechanisms in Some Single-Crystal Superalloys

Materials Science Forum, 2005
The creep behavior and microstructure of several nickel-base single-crystal superalloys after high-temperature low-stress creep have been investigated. These alloys were designed with varying content of the alloying elements Mo and Ru. At 1100°C and 137 MPa, the large g/g¢ lattice misfit in negative with the addition of Mo leads to the formation of ...
Yuichiro Koizumi, Hiroshi Harada
openaire   +1 more source

Creep fracture mechanisms in single crystal superalloys

Scripta Metallurgica et Materialia, 1992
cnr,itm,i-20092 cinisello balsamo,italy.;ai, sh (reprint author), acad sinica,inst met res,state key lab fatigue & fracture mat,shenyang 110015,peoples r ...
S.H Ai, V Lupinc, M Maldini
openaire   +1 more source

Multicycle Fatigue of Single Crystal Nickel Superalloy

Metallurgist, 2018
Multicycle fatigue of an experimental low-alloy single-crystal nickel-base superalloy is studied in relation to crystal orientation and test temperature. It is established that with an increase in test temperature from 20 to 900°C a change is observed in the shape of the multicycle fatigue curve.
M. S. Belyaev, M. R. Orlov
openaire   +1 more source