Results 71 to 80 of about 448,207 (186)
Solvent Debinding of MIM Parts in a Polystyrene-Palm Oil Based Binder System
Abstract The influence of the leaching temperatures on the solvent debinding process of SS316L stainless steel alloy compact has been investigated. Solvent debinding process of injection moulded SS316L feedstock was conducted to eliminate palm kernel oil by using n- heptane solution at various temperatures of 40, 50 and 60°C and at ...
R. Asmawi +3 more
openaire +1 more source
Advanced Manufacturing of Composite‐Based Systems for Energy Applications
Advanced manufacturing enables the integration of polymers, ceramics, metal oxides, and composites into architected microstructures with tailored transport pathways. By coupling material selection, manufacturing strategy, and structural design, multifunctional energy systems can simultaneously improve electrochemical performance, thermal management ...
Sri Vaishnavi Thummalapalli +13 more
wiley +1 more source
Fused granulate fabrication; Solvent-free thermal debinding; Alumina architectures; Triply periodic minimal surface (TPMS); Thermal shock resistance; Ammonia combustion reactor.
rong hua
core +1 more source
Recent Development of a High Performance Solid Oxide Electrolysis Cell at CEA
ABSTRACT This article focuses on two distinct methods for manufacturing an innovative solid oxide electrolysis cell and enhancing its electrochemical performances. On the hydrogen side, the support porosity was increased and optimized to prevent gas diffusion limitations at high current densities.
L. Guesnet, J. Bigarre, J. Vulliet
wiley +1 more source
Solvent debinding process in powder injection molding: experiments and numerical simulations
International audiencePowder Injection Molding (PIM) is a technology in which thermoplastic polymeric materials with a high content of metallic powders are molded in a required shape. In this paper, solvent debinding for copper green components shaped by
Gélin, Jean-Claude +2 more
core +1 more source
ABSTRACT The use of Ti6Al4V alloy in dental implantation is constrained by its high elastic modulus and biological inertness, which lead to delayed osseointegration and a high failure risk. Additionally, its chemical incompatibility with hydroxyapatite (HA) impedes the development of stable bioactive composites.
Shangyong Zuo +8 more
wiley +1 more source
Study of solvent debinding parameters for metal injection moulded 316L stainless steel
Solvent debinding is one of a crucial stage in Metal Injection Moulding (MIM) process. This process begins with the removal of the soluble binder components by using solvents such as heptane or hexane. In solvent debinding process, unsuccessful to achieve maximum binder removal will cause a defect to the compact such as crack and swelling.
M F F A Hamidi +4 more
openaire +1 more source
Focusing on the critical tap hole region of the blast furnace, this work examines binder characteristics, prepares tap hole clay with different formulations, and evaluates their physical properties. The findings confirm the advantages of composite binders and offer a new binder option for tap hole clay.
Frederik Tegeder +7 more
wiley +1 more source
Sustainable Debinding and Recovery of CO2-Soluble Binders
Metal and ceramic forming applications using conventional binders are associated with a number of environmental problems such as toxic emissions and carcinogenic wastes released from conventional binder removal processes.
Gulari, Esin +4 more
core +1 more source
ABSTRACT This study examined the effects of binder content and dispersion on aqueous ZrB2–SiC ceramic paste and the porosity of ZrB2–SiC ceramic parts fabricated using an extrusion‐based additive manufacturing process. An aqueous paste of ZrB2–SiC (70/30 by volume) powder with a 45 vol.% solids loading and hydroxypropyl methylcellulose as the binder ...
Abid H. Rafi +5 more
wiley +1 more source