Results 81 to 90 of about 448,207 (186)

Additive manufacturing of 17–4 PH steel using metal injection molding feedstock: Analysis of 3D extrusion printing, debinding and sintering

open access: yes, 2021
International audienceThe amalgamation of 3D extrusion printing (3DEP) and sintering results in a low-cost process compared to other laser-based additive manufacturing techniques. This work used metal injection molding (MIM) raw material of 17-4 PH steel
Bouvard, Didier   +7 more
core   +1 more source

Liquid-Phase Sintering and Properties of PIMed 10-20 vol.% SiCp-Reinforced Aluminium Composites

open access: yesMATEC Web of Conferences, 2018
Liquid-phase sintering and properties of powder injection moulded aluminium composite reinforced with SiCp has been investigated via thermal-phase analyses and hardness property.
Patcharawit Tapany   +3 more
doaj   +1 more source

The Effects of Nanoparticle Addition on Binder Removal from Injection Molded Aluminum Nitride [PDF]

open access: yes
The effects of nanoparticle addition on the multi-step debinding of injection molded aluminum nitride (AlN) samples were studied. Experiments varying the solvent debinding conditions (time, temperature and aspect ratio) were performed on monomodal ...
Onbattuvelli, Valmikanathan P.   +3 more
core   +3 more sources

Solvent Debinding of Injection Molded Fe-36% Ni with Use of Polyvinylbuthyral as Organic Binder.

open access: yesJournal of the Japan Society of Powder and Powder Metallurgy, 1993
It is necessary to reduce the debinding time in powder injection molding process. Therefore, recently, there are methods such as ANAX process of removing the binders and the solvent debinding which can solve the problems mentioned above becomes to get much attention.
Kankawa, Yoshimitsu   +3 more
openaire   +2 more sources

Supercritical debinding of environmentally friendly Inconel 718 feedstock to metal injection moulding process

open access: yes, 2016
International audienceIn the MIM process the debinding is a long, complicated and polluting step. The supercritical fluid debinding is a new method to reduce the time of debinding, the default of the pieces and the pollution.
Royer, Alexandre   +2 more
core  

Single Step of Binder Thermal Debinding and Sintering of Injection Moulded 316L Stainless Steel

open access: yes, 2010
Metal injection moulding was performed with gas atomized 316L stainless steel powders. Feedstocks were prepared using a paraffin wax/polyethylene/stearic acid binder system and subsequently molded into tensile bar specimens. Solvent extraction done at 80○
Indra Putra Almanar   +2 more
core   +1 more source

Benefits of supercritical CO₂ debinding for titanium powder injection moulding?

open access: yes, 2010
Supercritical CO₂ debinding has been described as a clean and environmentally friendly alternative to other debinding routes. The claims are that SC-CO₂ should prevent oxidation, lead to less defects and reduce the debinding time.
Thomas, Yannig, Baril, Éric
core   +1 more source

Debinding and Sintering of an Injection-Moulded Hypereutectic Al–Si Alloy

open access: yes, 2018
Hypereutectic Al–Si (20 wt.%) alloy parts were fabricated by employing a powder injection moulding (PIM) technique with a developed multi-component binder system composed of high-density polyethylene (35 wt.%), carnauba wax (62 wt.%) and stearic ...
Jiaqi Ni, Keqing Han, Muhuo Yu
core   +1 more source

Development of niobium powder injection molding. Part II: Debinding and sintering

open access: yes, 2019
This article is a continuation of feedstock preparation and powder injection molding (PIM) of pure niobium. Part II discusses debinding and sintering of injection molded niobium.
German, RM   +3 more
core   +1 more source

Effect of Solvent Debinding Process on the Properties of Fused Deposition Modelling 3D Printing Stainless Steel 316L

open access: yes
Metal 3D printing was considered expensive due to the high investment cost of the equipment (Powder bed technologies), as an approach to the FDM 3D printing process with fused metal filament at a lower cost, the metal used is 316L stainless steel.
Wiriyadinata, Dimas Aditiya
core  