Results 91 to 100 of about 20,532,860 (296)
Despite benefits to storage stability and handleability of aluminum scrap, octadecyl phosphonic acid (ODPA) SAMs reduce the tensile strength of wires produced using friction‐induced recycling. Etching and methyl diphosphonic acid (MDPA) coatings, however, have little effect.
Timothy D. Goller +3 more
wiley +1 more source
Crack is one of the main diseases of pavement structure. In order to improve the anti-reflective crack ability of pavement, fiber rubber gravel sealing layer is proposed as the stress absorbing layer.
Fujing Zhao (17827355) +3 more
core +1 more source
Enhancing the Flexural Characteristics of Stabilized Kaolinite Clay by Reinforcing with Composite Fiber [PDF]
In this research, a new type of fiber known as composite fibers has been utilized to enhance the flexural properties of stabilized clay. The core of the composite fiber consists of elastane, while its shell is composed of numerous polyester fibers.
Mahmood Reza Abdi +2 more
doaj +1 more source
Rotary 3D Printing With Integrated Electroplating
A rotary material extrusion platform integrates localized copper electroplating with printing and encapsulation to fabricate cylindrical polymer–metal structures containing fully embedded, low‐resistance conductive pathways that enable internal Joule heating and thermally activated shape‐memory responses.
Antonio Zagaria +5 more
wiley +1 more source
General introduction of the experimental methods of μCT and the three-point bending test.
(A) Experimental parameters of the rat tibia scanned using μCT. (B) Details on the experimental design of the three-point bending test consisting of an aluminum block and rounded edge-free notches.
Guo-Xian Chen (559691) +9 more
core +1 more source
Laser‐Induced Graphene from Waste Almond Shells
Almond shells, an abundant agricultural by‐product, are repurposed to create a fully bioderived almond shell/chitosan composite (ASC) degradable in soil. ASC is converted into laser‐induced graphene (LIG) by laser scribing and proposed as a substrate for transient electronics.
Yulia Steksova +9 more
wiley +1 more source
Power-law characteristics of damage and failure of ceramic coating systems under three-point bending
Damage and failure of ceramic coatings bonded on alloy substrates was studied by observing crack evolution in the coating systems under in situ three-point bending tests with corresponding load-displacement curves. A damage and catastrophic failure model
Liang, LH +5 more
core +1 more source
Effect of Coremat Xi 3 Middle Layer on Flexural Performance of Glass Fibre Composites under Different Test Rates [PDF]
This study presents experimental results from three-point bending tests conducted on two composite types reinforced with quadriaxial glass fibre fabrics, both using unsaturated polyester resin as matrix, and differing by the presence or absence of a ...
Ioana - Gabriela CHIRACU +5 more
doaj +1 more source
Shellac, a centuries‐old natural resin, is reimagined as a green material for flexible electronics. When combined with silver nanowires, shellac films deliver transparency, conductivity, and stability against humidity. These results position shellac as a sustainable alternative to synthetic polymers for transparent conductors in next‐generation ...
Rahaf Nafez Hussein +4 more
wiley +1 more source
Extracting nanowire mechanical properties from three-point bendig test
A new adhesive receding contact model is presented in this paper for the nanowire in three-point bending test. Because of its flexurality, the nanowire in test may lift-off/separate from its supporting elastic medium, which can dramatically change the ...
Liu Y, 张吟, Liu, Y.