Results 11 to 20 of about 3,391 (209)
Bio-tribocorrosion mechanisms in orthopaedic devices : mapping the micro-abrasion-corrosion behaviour of a simulated CoCrMo hip replacement in calf serum solution [PDF]
Load bearing implant prostheses such as orthopaedic hip and knee implants may be considered as tribocorrosion systems since the wear processes are a result of combined mechanical and chemical mechanisms.
Black, R.A., Stack, M.M., Sadiq, K.
core +4 more sources
Tribocorrosion of total hip replacements [PDF]
The performance of metal-on-metal total hip replacements is largely determined by their propensity to degrade in vivo. Degradation occurs through the complex interactions between wear and corrosion (termed tribocorrosion) and leads to the production of ...
Hesketh, James Edward Tilston
core +5 more sources
Degradation behavior of Ti-Nb alloys: Corrosion behavior through 21 days of immersion and tribocorrosion behavior against alumina [PDF]
Non-toxic and allergic free β-type Ti alloys are attractive metallic implant materials due to their lower Young's modulus and good biocompatibility, but the corrosion and tribocorrosion behavior are yet to be fully understood.
Pinto, A. M.P. +6 more
core +2 more sources
Tribocorrosion-Resistant Ti40Nb–TiN Composites Having TiO2‑Based Nanotubular Surfaces
A novel multifunctional material was developed by hard TiN particle reinforcement addition to a β-type Ti40Nb alloy, followed by surface functionalization, yielding the formation of a nanotubular layer.
Alexandra C. Alves +13 more
core +1 more source
Bio-Tribocorrosion of Titanium Dental Implants and Its Toxicological Implications: A Scoping Review
Bio-tribocorrosion is a phenomenon that combines the essentials of tribology (friction, wear, and lubrication) and corrosion with microbiological processes. Lately, it has gained attention in implant dentistry because dental implants are exposed to wear,
Sumit Gaur +2 more
doaj +1 more source
In this study, PEO coatings were produced on AZ91 Mg alloy using pulsed waveforms at different electrical parameters such as type (unipolar and bipolar), cathodic duty cycle (20 and 40 %), and voltage amplitude (350 and 400 V) to assess wear and ...
Ali Heydarian +4 more
doaj +1 more source
Sliding tribocorrosion behaviours of AISI 316 stainless steel were investigated against alumina ball in natural seawater environment (SWE) under 5 N loads.
Sabri Alkan, Mustafa Sabri Gök
doaj +1 more source
Progression of Bio-Tribocorrosion in Implant Dentistry
Oral rehabilitation devices are susceptible to bio-tribocorrosion phenomena in the oral environment due to the synergism of wear, chemical, biochemical, and microbiological processes.
Caroline Dini +5 more
doaj +1 more source
The evolution of microstructures and the mechanical properties of the fabricated compacts were analyzed following pulsed electric current sintering (PECS) of ceramics reinforced titanium samples. The Vickers microhardness values of the fabricated samples
Olusoji Oluremi Ayodele +2 more
doaj +1 more source
Corrosion and tribocorrosion behaviour of titanium nitride thin films grown on titanium under different deposition times [PDF]
Ti and its alloys exhibit combination of unique properties for biomedical applications, however their poor tribo-electrochemical behaviour is a major concern.
Rocha, L. A. [UNESP] +16 more