Fail-Safe Joints between Copper Alloy (C18150) and Nickel-Based Superalloy (GH4169) Made by Transient Liquid Phase (TLP) Bonding and Using Boron-Nickel (BNi-2) Interlayer [PDF]
Joining heat conducting alloys, such as copper and its alloys, to heat resistant nickel-based superalloys has vast applications in nuclear power plants (including future fusion reactors) and liquid propellant launch vehicles.
Shirzadi, Amir A., Zhang, Chencong
core +3 more sources
Effects of returns on composition, microstructure and mechanical properties of GH4169 superalloy [PDF]
To recycle the returned alloy effectively, effects of returns proportion on alloy composition, microstructure and compression properties of superalloy GH4169 were studied by means of scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS)
Yong-liang Pu +2 more
doaj +3 more sources
Investigation on White Layer Formation in Dry High-Speed Milling of Nickel-Based Superalloy GH4169 [PDF]
To investigate the formation mechanism of the white layer on the machined surface during high-speed milling of nickel-based superalloy GH4169, several cutting parameters were selected for milling experiments.
Jiamao Zhang +3 more
doaj +2 more sources
Regenerative Chatter Evaluation when Turning Nickel-based Superalloy GH4169 Using PCBN Cutting Tool [PDF]
Vibration during machining operation is a major issue that lowers cutting operation efficiency. Usually high cutting forces are encountered during machining processes, consequently shortening cutting tool lifetime.
Fadul Almula, Mubarak A.M. +2 more
core +3 more sources
Influence of precipitates on the initial oxidation behavior of GH4169 superalloy at 1000 °C
The degradation of mechanical properties in superalloys due to high temperature oxidation is unavoidable. In this paper, the initial oxidation (oxidation time less than 3600 s) mechanism of GH4169 superalloy was studied.
Lei Yin +8 more
doaj +2 more sources
Study on surface quality of GH4169 superalloy milling with ultrasonic synergistic nanofluid minimal quantity lubrication [PDF]
GH4169 superalloy is extensively utilized in aerospace applications due to their exceptional high-temperature strength and oxidation resistance properties.
Xuezhi Wang +4 more
doaj +2 more sources
Effects of Pulse Current on Dynamic Recrystallization Behavior of GH4169 Superalloy
The pulse current was applied on the GH4169 alloy during tensile tests at 800°C. The effects of pulse current on the deformation behavior and recrystallization of the alloy were investigated, and the mechanisms were also discussed. The results show that the deformation resistance decreases and the elongation increases significantly by applying the ...
Yang Liu +4 more
openaire +3 more sources
Surface Microstructure of Nanoaluminized CoCrAlY Coating Irradiated by HCPEB [PDF]
A thermal sprayed CoCrAlY coating was prepared by air plasma spray on the surface of Ni-based superalloy GH4169; then, a nanoscale aluminum film was deposited with electron beam vacuum deposition on it.
Jian Han, Zhenzhu Jing, Zhiyong Han
core +3 more sources
Influence of pass spacing on the spinning process of nickel-based alloy conical casing [PDF]
High temperature nickel-based alloys are prone to forming defects due to serious work hardening, and the pass spacing is an important parameter in multi-pass drawing and spinning.
L. Ding +4 more
doaj +1 more source
Influence of ZnO Film Deposition Parameters on Piezoelectric Properties and Film-to-Substrate Adhesion on a GH4169 Superalloy Steel Substrate. [PDF]
Mo G, Cui Y, Yin J, Gao P.
europepmc +3 more sources