Results 81 to 90 of about 220,287 (359)
14‐day casting‐induced immobilization reduced gastrocnemius muscle mass and increased non‐heme iron and ferritin heavy chain levels. Despite iron accumulation, transferrin receptor 1 and iron regulatory protein 2 were paradoxically upregulated. Lipid peroxidation was elevated without compensatory antioxidant responses.
Haruka Yokogawa +2 more
wiley +1 more source
Laser additive manufacturing of Mg-based composite with improved degradation behaviour
Magnesium (Mg) alloy shows great potential as bone implant owing to its favourable biocompatibility and degradability. In the present work, bioglass-reinforced Mg-based composite was manufactured via laser additive manufacturing.
Youwen Yang +6 more
doaj +1 more source
Rheo-diecasting AZ91D magnesium alloy [PDF]
Magnesium recycling has become more important in today’s environmentally aware society. To prompt the usage of recycled magnesium scrap and further improve casting structure and properties, a novel physical approach, the rheo-diecasting process (RDC ...
Fan, Z, Liu, G, Wang, Y
core
Abruptly changing from aerobic to anaerobic conditions (sudden anaerobization) induced growth inhibition and a significant increase in intracellular labile ferrous iron in the aerotolerant anaerobe Amphibacillus xylanus. We found that free flavins mediate efficient electron transfer from NADH to ferric iron under anaerobic conditions, suggesting that ...
Shinya Kimata +13 more
wiley +1 more source
Analysis of precipitation and dissolution in overaged 7xxx aluminium alloys using DSC
To improve the understanding of the relation between composition, precipitation and the balance of strength and electrical conductivity (as a measure of the stress-corrosion resistance), a number of Al Zn Mg Cu Zr aluminium alloy plates with different Zn,
Li, Xiaomei, Starink, M.J.
core +1 more source
ErB4 and NdB4 nanostructured powders are produced by mechanochemical synthesis. 5 h mechanical alloying and 4 M HCl acid leaching are used in the production. ErB4 and NdB4 powders exhibit maximum magnetization of 0.4726 emu g−1 accompanied with an antiferromagnetic‐to‐paramagnetic phase transition at about TN = 18 K and 0.132 emu g−1 with a maximum at ...
Burçak Boztemur +5 more
wiley +1 more source
Phase-field simulation for anisotropic dendrite growth in Mg-3wt.%Zn alloy
The anisotropy interfacial energy changes the growth tendency of dendrites in different directions during solidification, when the growth tendency in a specific direction appears or disappears, the transition of dendrite orientation will happen.
Kaixin Sun +4 more
doaj +1 more source
Grain refinement in a AlZnMgCuTi alloy by intensive melt shearing: A multi-step nucleation mechanism [PDF]
This is a post-print version of the article. Copyright @ 2010 Elsevier B.V.Direct chill (DC) cast ingots of wrought Al alloys conventionally require the deliberate addition of a grain refiner to provide a uniform as-cast microstructure for the ...
Cao +35 more
core +1 more source
The stability criteria affecting the formation of high‐entropy alloys, particularly focusing in supersaturated solid solutions produced by mechanical alloying, are analyzed. Criteria based on Hume–Rothery rules are distinguished from those derived from thermodynamic relations. The formers are generally applicable to mechanically alloyed samples.
Javier S. Blázquez +5 more
wiley +1 more source
FSW between Al alloy and Mg Alloy: the comparative study
It is difficult to fusion weld Al alloy to Mg alloy, so by experimental optimization procedure (EOP) optimum parameters for FSW between Al alloy and Mg alloy were determined and experiment conducted using these parameters resulted in not only sound weld ...
Jagadeesha C. B.