The parameters of electrolytic synthesis of Ni-P coatings on steel surface from sulfate-chloride electrolyte have been determinated. The Ni-P alloys consist of separate phases of Ni and Ni3P and solid solution of implementation on the basis of the FCC Ni
Vadim Chayevski, Valerij Zhylinski
doaj +1 more source
Molybdenum coatings due to their excellent wear resistant properties and sliding characteristics under dry friction conditions are often used in applications to resist friction and dry sliding.
Mrdak, Mihailo +8 more
core +1 more source
Mikrostruktura materijala za dijalizatore
Hemodijaliza je izvantjelesni postupak kojim se u medicini nastoji pomoću polupropusnih membrana u uređajima za hemodijalizu ukloniti uremijske toksine. Ovaj diplomski rad donosi pregled mehanizama kojima se uklanjaju uremijski toksini te pregled materijala koji se koriste za izradu polupropusnih membrana i postupaka proizvodnje kojima se membrane ...
openaire +1 more source
At present the durability of engineering structures built of high performance cement concrete constitutes a very important issue especially when we consider the reliability of these structures under the impact of different classes of aggressive ...
Michał Michał +2 more
doaj +1 more source
Mikrostruktura, lejność, stabilność mikrostruktury i właściwości mechaniczne stopu magnezu ZRE1 [PDF]
The influence of pouring temperature on the microstructure, fluidity and mechanical properties of ZRE1 magnesium alloy was investigated in this paper.
Rzychoń, T., Szala, J., Kiełbus, A.
core
The paper presents two part investigation into the behaviour of poly- and monodispersed granular material applying the discrete element method (DEM). Granular aggregates involve the compaction of spherical particles within the wall-bounded domain under ...
Gvidas Pocius, Robertas Balevičius
doaj +1 more source
Mikrostruktura i mehanička svojstva legure Inconel 625 pri aditivnoj proizvodnji električnim lukom i žicom [PDF]
U ovome je radu opisan postupak aditivne proizvodnje električnim lukom i žicom te je detaljnije obrađeno MAG zavarivanje i prikladni modaliteti prijenosa metala u električnom luku.
Sinković, Martin
core
Mikrostruktura i właściwości mechaniczne powłok kompozytowych (WC-Co+Co) natryskiwanych metodą HVOF na żeliwo sferoidalne [PDF]
An investigation was conducted to determine the role of Co particles in the WC-Co coating produced with the High Velocity Oxygen-Fuel (HVOF) spraying on microstructure, mechanical and wear properties in a system of type: WC-Co coating/ductlile cast iron.
Ksiazek, Marzanna +3 more
core +1 more source
The article deals with the flame sprayed Ni-Cr and Ni-Cr-WC coatings on construction S235 steel substrates. Before spraying, the surfaces of substrates were treated mechanically.
Ovidijus Jarašūnas +1 more
doaj +1 more source
Mikrostruktura i svojstva duplex (C + N) slojeva
This paper presents an examination of the wear resistance of a duplex thermodiffusion (C+N) layer in the erosion–corrosion conditions. Two low-carbon steels for carburizing C15E (Č1221) and 16MnCr5 (Č4320) have been selected for a combined surface hardening treatment with carbon and nitrogen.