Results 231 to 240 of about 46,916 (258)
Some of the next articles are maybe not open access.
Grease effect on fretting wear of mild steel
Industrial Lubrication and Tribology, 2008Purpose – The aim of this paper is to research grease and additives' influence on fretting wear of mild steel.Design/methodology/approach – Experiments were performed on a laboratory stand with contact conditions cylinder on flat. The mild steel couples were tested under dry conditions and lubricated with mineral and synthetic greases containing as ...
Antoni Neyman, Jan Sikora
openaire +1 more source
Tire Wear Caused by Mild Tread Slip
Rubber Chemistry and Technology, 1997Abstract The purpose of this study is to examine the relationship between the tread wear of rolling tires and the wear of a sliding rubber pad. In the experiments, frictional parameters, i.e. sliding distances, sliding velocities, and contact pressures, are evaluated at points on the tire-tread surface.
Tatsuo Fujikawa +2 more
openaire +1 more source
The unlubricated fretting wear of mild steel in air
Wear, 1985Abstract Fretting experiments were carried out on mild steel in air to long sliding distances over a range of loads and stroke amplitudes. For peak-to-peak fretting amplitudes greater than 5 μm, three fretting stages were identified: an initial adhesive transfer stage, an intermediate stage where both metallic and oxide debris were produced and a ...
D. Aldham, J. Warburton, R.E. Pendlebury
openaire +1 more source
Reaction products in and around the wear track in the lubricated mild wear regime
Wear, 1984Abstract Liquid or solid reaction products that are insoluble in the lubricant and the metallic wear debris generated in the wear track are partially deposited around the wear track where they can be easily studied after experiments. A ball-on-plate friction apparatus operating in the mild wear regime is used for investigating these deposits and the ...
openaire +1 more source
Wear resistance of plasma coatings on mild steel
Journal of Materials Science, 1991Mild steel was coated by different materials using plasma spray technique. Materials used as coatings are Ni-5% Al and WC-17% Co. The thickness of the coatings varied between 0.05 to 1.5 mm. The porosity of different coatings decreased with increase in thickness of the coat. The roughness of coating material decreased after wear testing. Microstrueture
M. M. I. Ahmed +4 more
openaire +1 more source
Mild microscopic wear in the boundary lubrication regime
Materialwissenschaft und Werkstofftechnik, 2010AbstractThe transition from a mild wear situation to a severe (adhesive) wear situation is of great interest to be able to design highly loaded concentrated contacts operating in the boundary lubricated regime. In this article a method is described to estimate this transition, based on a thermal criterion.
openaire +2 more sources
An experimental analysis of a mild wear process
2013U.S. Navy (U.S.N.) authors.
Barrett, Roy Franklin +1 more
openaire +1 more source
Some microscopic aspects of the mild wear of steel*
Journal of Microscopy, 1971SUMMARYThe paper reviews the experimental classifications of the unlubricated sliding wear of metals, together with some of the suggested relationships between the wear rates, the real area of contact, the load, the hardnesses of the metals and the probability of producing wear particles at the real areas of contact.
openaire +1 more source
A study of some aspects of a mild wear process
2012http://archive.org/details ...
Boyd, John Huntly. +2 more
openaire +1 more source